The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 15, 2025

Filed:

Jul. 17, 2023
Applicant:

Posco Co., Ltd, Pohang-si, KR;

Inventors:

Tae-Jin Song, Gwangyang-si, KR;

Min-Seo Koo, Gwangyang-si, KR;

Assignee:

POSCO CO., LTD, Pohang-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/04 (2006.01); B23K 20/04 (2006.01); B23K 20/227 (2006.01); B23K 20/24 (2006.01); B23K 31/02 (2006.01); B32B 15/01 (2006.01); B32B 15/18 (2006.01); B32B 38/00 (2006.01); C21D 1/18 (2006.01); C21D 8/02 (2006.01); C21D 8/04 (2006.01); C21D 9/46 (2006.01); C21D 9/48 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/18 (2006.01); C22C 38/22 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01); C22C 38/32 (2006.01); C22C 38/34 (2006.01); C22C 38/38 (2006.01); C22C 38/40 (2006.01); C22C 38/44 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/54 (2006.01); C23C 2/02 (2006.01); C23C 2/06 (2006.01); C23C 2/12 (2006.01); C23C 2/18 (2006.01); C23C 2/34 (2006.01); C23C 2/40 (2006.01); C23C 30/00 (2006.01); B23K 101/16 (2006.01); B23K 101/18 (2006.01); B23K 103/04 (2006.01); B23K 103/18 (2006.01); C21D 1/25 (2006.01); C22C 38/04 (2006.01);
U.S. Cl.
CPC ...
B32B 38/004 (2013.01); B23K 20/04 (2013.01); B23K 20/227 (2013.01); B23K 20/24 (2013.01); B23K 31/02 (2013.01); B32B 15/01 (2013.01); B32B 15/011 (2013.01); B32B 15/015 (2013.01); B32B 15/04 (2013.01); B32B 15/043 (2013.01); B32B 15/18 (2013.01); C21D 1/18 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/041 (2013.01); C21D 8/0426 (2013.01); C21D 8/0436 (2013.01); C21D 8/0463 (2013.01); C21D 8/0473 (2013.01); C21D 9/48 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/18 (2013.01); C22C 38/22 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); C22C 38/34 (2013.01); C22C 38/38 (2013.01); C22C 38/40 (2013.01); C22C 38/44 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01); C23C 2/02 (2013.01); C23C 2/022 (2022.08); C23C 2/024 (2022.08); C23C 2/026 (2022.08); C23C 2/06 (2013.01); C23C 2/12 (2013.01); C23C 2/18 (2013.01); C23C 2/34 (2013.01); C23C 2/40 (2013.01); C23C 30/00 (2013.01); C23C 30/005 (2013.01); B23K 2101/16 (2018.08); B23K 2101/18 (2018.08); B23K 2103/04 (2018.08); B23K 2103/18 (2018.08); B32B 15/012 (2013.01); B32B 15/013 (2013.01); B32B 2038/0048 (2013.01); B32B 2250/03 (2013.01); B32B 2250/40 (2013.01); B32B 2307/536 (2013.01); B32B 2307/552 (2013.01); B32B 2307/72 (2013.01); C21D 1/25 (2013.01); C21D 2211/001 (2013.01); C21D 2211/002 (2013.01); C21D 2211/004 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01); C21D 2251/02 (2013.01); C22C 38/04 (2013.01); Y10T 428/12451 (2015.01); Y10T 428/12493 (2015.01); Y10T 428/12729 (2015.01); Y10T 428/12757 (2015.01); Y10T 428/12799 (2015.01); Y10T 428/12958 (2015.01); Y10T 428/12965 (2015.01); Y10T 428/12972 (2015.01); Y10T 428/12979 (2015.01); Y10T 428/12993 (2015.01); Y10T 428/2495 (2015.01); Y10T 428/24959 (2015.01); Y10T 428/24967 (2015.01); Y10T 428/24992 (2015.01); Y10T 428/26 (2015.01); Y10T 428/263 (2015.01); Y10T 428/264 (2015.01); Y10T 428/265 (2015.01);
Abstract

Provided is a method of manufacturing a clad steel sheet. The method includes: preparing a base material including C: 0.3 to 1.0%, Mn: 4.0 to 16.0%, Al: 4.5 to 9.0%, and a remainder of Fe and inevitable impurities; preparing a cladding material including C: 0.1 to 0.45%, Mn: 0.1 to 3.0%, and a remainder of Fe and inevitable impurities; disposing the base material between two of the cladding material to obtain a laminate; welding an edge of the laminate; heating the welded laminate between 1050 and 1350° C.; finish-rolling the heated laminate between 750 and 1050° C. with a rolling reduction ratio of 30% or more in a first pass; coiling the hot-rolled steel sheet between 400 and 700° C.; pickling the coiled hot-rolled steel sheet, and applying a cold-reduction ratio of 35 to 90%; and annealing the cold-rolled steel sheet between 550° C. and A3+200° C. of the cladding material.