The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 15, 2025

Filed:

May. 25, 2023
Applicant:

Nan Ya Plastics Corporation, Taipei, TW;

Inventors:

Wen-Cheng Yang, Taipei, TW;

Te-Chao Liao, Taipei, TW;

Hao-Sheng Chen, Taipei, TW;

Chien-Chih Lin, Taipei, TW;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B29C 48/19 (2019.01); B29B 7/14 (2006.01); B29C 48/40 (2019.01); B32B 27/08 (2006.01); B32B 27/20 (2006.01); B32B 27/36 (2006.01); C08J 3/22 (2006.01); B29K 67/00 (2006.01);
U.S. Cl.
CPC ...
B29C 48/19 (2019.02); B29B 7/14 (2013.01); B29C 48/40 (2019.02); B32B 27/08 (2013.01); B32B 27/20 (2013.01); B32B 27/36 (2013.01); C08J 3/22 (2013.01); B29K 2067/00 (2013.01); B29K 2995/0016 (2013.01); B29K 2995/0039 (2013.01); B29K 2995/004 (2013.01); B29K 2995/0041 (2013.01); B32B 2250/02 (2013.01); B32B 2250/03 (2013.01); B32B 2307/306 (2013.01); C08J 2367/00 (2013.01); C08J 2471/00 (2013.01); C08J 2479/08 (2013.01); C08J 2481/06 (2013.01);
Abstract

A method for producing a polyester film is provided. The method includes a resin alloy master batch preparation step and a film forming step. The resin alloy master batch preparation step includes melting and kneading a high temperature resistant resin material and a polyester resin material with a twin-screw granulator, and then forming a plurality of resin alloy master batches. In the resin alloy master batch preparation step, a twin-screw temperature of the twin-screw granulator is between 250° C. and 320° C., and a twin-screw rotation speed of the twin-screw granulator is between 300 rpm and 800 rpm. The film forming step includes melting and extruding the resin alloy master batches with to form a polyester film. The polyester film includes a heat resistant layer formed of the plurality of resin alloy master batches so that the heat resistant layer includes the high temperature resistant resin material and the polyester resin material.