The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 08, 2025

Filed:

May. 20, 2021
Applicant:

P.t. Medisafe Technologies, Medan, ID;

Inventors:

Monichan Puthuvelil Mathew, Kuala Lumpur, MY;

Asish Kumar Sharma, Medan, ID;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K 5/3445 (2006.01); A41D 19/00 (2006.01); A61B 42/10 (2016.01); C08J 5/02 (2006.01); C08K 3/22 (2006.01); C08L 9/04 (2006.01); C08L 9/08 (2006.01); C08L 9/10 (2006.01); C08L 11/02 (2006.01); C08L 13/00 (2006.01); C08L 79/00 (2006.01);
U.S. Cl.
CPC ...
C08K 5/3445 (2013.01); A41D 19/0082 (2013.01); A61B 42/10 (2016.02); C08J 5/02 (2013.01); C08K 3/22 (2013.01); C08L 9/04 (2013.01); C08L 9/08 (2013.01); C08L 9/10 (2013.01); C08L 11/02 (2013.01); C08L 13/00 (2013.01); C08L 79/00 (2013.01); C08J 2309/04 (2013.01); C08J 2309/08 (2013.01); C08J 2309/10 (2013.01); C08J 2311/02 (2013.01); C08J 2313/02 (2013.01); C08K 2003/2227 (2013.01); C08K 2003/2296 (2013.01); C08L 2201/52 (2013.01); C08L 2203/02 (2013.01);
Abstract

Provided are compositions and associated methods for producing elastomeric rubber gloves with improved strength and flexibility at desirable glove palm thicknesses. An example elastomeric rubber glove comprises a substrate formed from a composition comprising a synthetic rubber latex, and an ionic liquid. The ionic liquid may comprise a combination of one or more alkyl imidazole ionic salts. The composition may comprise one or more metal oxides, including at least one of zinc oxide, magnesium oxide, cadmium oxide, and aluminum oxide. The synthetic rubber latex compositions were found to yield a material with strength and flexibility characteristics comparable to natural latex gloves of a greater thickness. The described gloves may also be cured without the addition of Sulphur and other vulcanization or rubber accelerators, further reducing the risk of allergies and costs of production.