The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jul. 01, 2025
Filed:
Nov. 19, 2024
Changzhou University, Jiangsu, CN;
Xiazhang Li, Changzhou, CN;
Taoli Huhe, Changzhou, CN;
Shixiang Zuo, Changzhou, CN;
Xiaofei Yin, Changzhou, CN;
Xiaoshan Meng, Changzhou, CN;
Chao Yao, Changzhou, CN;
Bingying Gao, Changzhou, CN;
CHANGZHOU UNIVERSITY, Changzhou, CN;
Abstract
A method for preparing two-dimensional sheet-like LiSiOsorbent, including: obtaining LiCoOby performing discharging, aluminum foil stripping, and sieving on waste lithium battery cathode material, and drying; obtaining biomass by freeze-drying waste biomass, and grinding and sieving the freeze-dried waste biomass; mixing LiCoOand the biomass uniformly to obtain a mixture, and putting the mixture into a tube furnace for nitrogen purging, heating and calcination, and carbothermal reduction to obtain a solid sample, hydrothermal stirring the solid sample, followed by filtering, and evaporating to obtain LiCO; ultrasonically dispersing the attapulgite in an acid solution, and stirring in a water bath at 80° C. to obtain a first product, washing the first product until neutrality, filtering, and drying overnight to obtain SiO; and ultrasonically dispersing the weighed SiOin deionized water, adding NaOH for hydrothermal stirring, adding the obtained LiCOfor stirring reaction, adding NHF, and dropwise adding ammonia water to adjust pH of a solution, transferring the solution to a microwave hydrothermal reaction kettle for microwave hydrothermal reaction to obtain a second product, and centrifuging, washing, drying, and calcining the second product to obtain the two-dimensional sheet-like LiSiO.