The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 01, 2025

Filed:

Sep. 27, 2017
Applicant:

Nitto Denko Corporation, Ibaraki, JP;

Inventors:

Satoru Suzuki, Ibaraki, JP;

Tomoya Ogawa, Ibaraki, JP;

Tomonari Naito, Ibaraki, JP;

Naoki Kurata, Ibaraki, JP;

Satomi Yoshie, Ibaraki, JP;

Kohei Nagao, Ibaraki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B08B 17/02 (2006.01); B05D 5/00 (2006.01); B05D 7/00 (2006.01); B05D 7/02 (2006.01); B63B 59/04 (2006.01); C09D 5/16 (2006.01); C09D 5/20 (2006.01); C09D 153/02 (2006.01); C09D 183/04 (2006.01); E02B 17/00 (2006.01); E02D 29/09 (2006.01);
U.S. Cl.
CPC ...
B08B 17/02 (2013.01); B05D 5/00 (2013.01); B05D 7/02 (2013.01); B05D 7/544 (2013.01); B63B 59/04 (2013.01); C09D 5/1675 (2013.01); C09D 5/1693 (2013.01); C09D 5/20 (2013.01); C09D 153/025 (2013.01); C09D 183/04 (2013.01); E02B 17/0026 (2013.01); E02D 29/06 (2013.01); E02D 2300/0001 (2013.01); E02D 2300/0006 (2013.01); E02D 2300/0025 (2013.01);
Abstract

A coating film capable of being peeled off in the shape of sheet to facilitate a coating film removal work, and is less likely to peel even after long periods of use on an underwater structure is provided. The coating film comprises an undercoat layer to be bonded to an underwater structure, and an antifouling layer bonded to the undercoat layer, wherein: a 100-gram underwater constant load peeling degree of the coating film is less than 5; a ratio of a tensile breaking strength of the coating film to an adhesive force of the coating film with respect to the underwater structure, as measured after immersing the coating film in pure water at 60° C. for 5 weeks is 1.5 or more; and a 1-mm square cross-cut stretching-caused peeling degree of the antifouling layer with respect to the undercoat layer is 0.05 or less.