The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 24, 2025

Filed:

Aug. 25, 2020
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Takuya Hirashima, Tokyo, JP;

Shimpei Yoshioka, Tokyo, JP;

Shinjiro Kaneko, Tokyo, JP;

Soshi Yoshimoto, Tokyo, JP;

Tomohiro Hashimukai, Tokyo, JP;

Yoshihiko Ono, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C21D 1/18 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 1/18 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/38 (2013.01);
Abstract

A steel sheet having a steel microstructure including, by area %, martensite in a range of 20% or more and 100% or less, ferrite in a range of 0% or more and 80% or less, and the balance being 5% or less. A residual stress generated at the transverse center of the steel sheet when the steel sheet is subjected to a V-bending process is 800 MPa or less. A residual stress generated at the transverse end of the steel sheet when the steel sheet is subjected to a V-bending process is 90% or more and 110% or less of the residual stress generated at the transverse center of the steel sheet. The maximum amount of warpage of the steel sheet sheared to a length of 1 m in the longitudinal direction is 15 mm or less.