The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 17, 2025

Filed:

Apr. 19, 2021
Applicant:

Nippon Paper Industries Co., Ltd., Tokyo, JP;

Inventors:

Tomohiro Okeda, Tokyo, JP;

Takato Takenaka, Tokyo, JP;

Isamu Ono, Tokyo, JP;

Minoru Yada, Tokyo, JP;

Hiroko Iwakiri, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 20/18 (2006.01); B32B 15/085 (2006.01); B32B 15/20 (2006.01); B32B 27/32 (2006.01); C08F 8/46 (2006.01); C08F 255/02 (2006.01); C09D 11/106 (2014.01); C09D 151/06 (2006.01);
U.S. Cl.
CPC ...
C08F 20/18 (2013.01); C08F 8/46 (2013.01); C08F 255/02 (2013.01); C09D 11/106 (2013.01); C09D 151/06 (2013.01); B32B 15/085 (2013.01); B32B 15/20 (2013.01); B32B 27/32 (2013.01); B32B 2255/06 (2013.01); B32B 2255/26 (2013.01);
Abstract

An object of the present invention is to provide a modified polyolefin resin composition having a high polyethylene content and exhibiting a good balance between a low-temperature stability and an adhesion to a polyethylene substrate and a metal. The present invention provides a modified polyolefin resin that is a graft-modified product in which a component (A) that is a polyolefin resin having an ethylene structural unit content of 50% or more by mole is modified with a component (B) that is an α,β-unsaturated carboxylic acid or an anhydride thereof and a component (C) that is a (meth)acrylate ester represented by the following general formula (I), and an extrapolated melting end temperature (Tem) of the modified polyolefin resin measured in accordance with JIS K7121-1987 using a differential scanning calorimeter at a temperature raising rate of 10° C./minute is 58° C. or lower.