The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jun. 10, 2025
Filed:
Jul. 31, 2023
PT Esg New Energy Material, Jakarta, ID;
PT Qmb New Energy Materials, Jakarta, ID;
Gem Co., Ltd., Shenzhen, CN;
PT Gem Indonesia New Energy Materials, Jakarta, ID;
Satryo Soemantri Brodjonegoro, Jakarta, ID;
Kaihua Xu, Shenzhen, CN;
Rizky Wanaldi, Jakarta, ID;
Tegar Mukti Aji, Jakarta, ID;
Aad Alief Rasyidi Baking, Jakarta, ID;
Andi Syaputra Hasibuan, Jakarta, ID;
Piyan Rahmadi, Jakarta, ID;
Wei Liu, Jakarta, ID;
PT ESG NEW ENERGY MATERIAL, Jakarta, ID;
PT QMB NEW ENERGY MATERIALS, Jakarta, ID;
GEM CO., LTD., Shenzhen, CN;
PT GEM INDONESIA NEW ENERGY MATERIALS, Jakarta, ID;
Abstract
A treatment method and application for laterite nickel ore leaching solution with high calcium and magnesium content, comprising the following steps: S1. preparing an extracted organic phase from the 2-hexyldecanoic acid and the HBL110/HBL116 extractant; S2. performing nickel-cobalt co-extraction on the extracted organic phase and a laterite nickel ore leaching solution with a high calcium and magnesium content to obtain a first loaded organic phase and a raffinate; in a laterite nickel ore leaching solution with a high calcium and magnesium content; S3. washing the first loaded organic phase with a washing solution to obtain a second loaded organic phase and washing water, wherein the washing water is refluxed to a laterite nickel ore leaching solution with high calcium and magnesium content; S4. adding a reverse extracting solution to the second loaded organic phase for reverse extracting to obtain a nickel-cobalt salt solution and a reverse extracted organic phase; S5. saponifying the reverse extracted organic phase to obtain a regenerated extracted organic phase; this scheme is applicable to the environment with high calcium and magnesium, can prevent calcium and magnesium from forming a third phase, and the effect of separating and purifying nickel and cobalt is good.