The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 27, 2025

Filed:

Jun. 26, 2020
Applicant:

Pulpac Ab, Västra Frölunda, SE;

Inventors:

Edward Guidotti, Gothenburg, SE;

Mostafa Jabbari, Västra Frölunda, SE;

Assignee:

PULPAC AB, Västra Frölunda, SE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D21H 19/82 (2006.01); B31B 50/14 (2017.01); B31B 50/59 (2017.01); B31B 120/00 (2017.01); D04H 1/26 (2012.01); D04H 1/425 (2012.01); D04H 1/732 (2012.01); D21H 19/16 (2006.01); D21H 19/20 (2006.01); D21H 21/16 (2006.01);
U.S. Cl.
CPC ...
D21H 19/824 (2013.01); B31B 50/142 (2017.08); B31B 50/592 (2018.05); D04H 1/26 (2013.01); D04H 1/425 (2013.01); D04H 1/732 (2013.01); D21H 19/16 (2013.01); D21H 19/20 (2013.01); D21H 21/16 (2013.01); B31B 2120/00 (2017.08);
Abstract

A method for producing a cellulose product from an air-formed cellulose blank structure comprising the steps of: providing a cellulose blank structure which is air-formed from cellulose fibres; applying, in a first application step (S), an alkyl ketene dimer (AKD) dispersion to the cellulose blank structure, and applying, in a second application step (S) a latex dispersion to the cellulose blank structure arranging the cellulose blank structure with the applied alkyl ketene dimer (AKD) dispersion and latex dispersion in a forming mould; heating the cellulose blank structure to a forming temperature (T) in the range of 100° C. to 300° C., and forming the cellulose product from the cellulose blank structure in the forming mould, by pressing the heated cellulose blank structure with the applied alkyl ketene dimer (AKD) dispersion and latex dispersion with a forming pressure (P) of at least 1 MPa, preferably 4-20 MPa.