The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
May. 20, 2025
Filed:
Feb. 13, 2020
Nippon Steel Corporation, Tokyo, JP;
Usui Co., Ltd., Shizuoka, JP;
Taizo Makino, Tokyo, JP;
Masahiro Yamazaki, Tokyo, JP;
Tomohiko Omura, Tokyo, JP;
Yuji Arai, Tokyo, JP;
Osamu Endo, Shizuoka, JP;
Naoki Serizawa, Shizuoka, JP;
Tatsuya Masuda, Shizuoka, JP;
NIPPON STEEL CORPORATION, Tokyo, JP;
USUI CO., LTD., Shizuoka, JP;
Abstract
A steel pipe for a fuel injection pipe has a chemical composition consisting of, by mass %: C: 0.17 to 0.27%, Si: 0.05 to 0.40%, Mn: 0.30 to 2.00%, P: 0.020% or less, S: 0.0100% or less, O: 0.0040% or less, Ca: 0.0010% or less, Al: 0.005 to 0.060%, N: 0.0020 to 0.0080%, Ti: 0.005 to 0.015%, Nb: 0.015 to 0.045%, Cr: 0 to 1.00%, Mo: 0 to 1.00%, Cu: 0 to 0.50%, Ni: 0 to 0.50%, V: 0 to 0.15%, and the balance: Fe and impurities. The metal micro-structure consists substantially of tempered martensite, or tempered martensite and tempered bainite. The hardness is within the range of 350 to 460 HV1. A lattice spacing of a (211) diffraction plane measured by CoKα characteristic X-ray diffraction is 1.1716 Å or less, and a half-value width of the (211) diffraction plane is 1.200° or less. The number density of cementite having a diameter of 50 nm or more is 20/μmor less.