The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 20, 2025

Filed:

Jul. 15, 2021
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Eriko Tsukamoto, Tokyo, JP;

Kengo Takeda, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/01 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/60 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/013 (2013.01); C21D 6/001 (2013.01); C21D 6/005 (2013.01); C21D 6/007 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0263 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/60 (2013.01); C21D 2211/001 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

This steel sheet has a predetermined chemical composition, the metallurgical structure at a thickness ¼ portion is, by area ratio, martensite: 40% to 97%, ferrite+bainite: 50% or less, residual austenite: 3% to 20% and a remainder in microstructure: 5% or less, the aspect ratio of residual austenite having an aspect ratio of 3 or more is 80% or more with respect to the total area of residual austenite, and the number of carbides having a grain diameter of 8 to 40 nm per square micrometer is five or more in the residual austenite.