The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 13, 2025

Filed:

Dec. 08, 2020
Applicant:

Owens Corning Intellectual Capital, Llc, Toledo, OH (US);

Inventors:

Gert Mueller, New Albany, OH (US);

Andrew Broderick, Newark, OH (US);

Xiujuan Zhang, New Albany, OH (US);

Liang Chen, New Albany, OH (US);

Kendel Smith, Westerville, OH (US);

Larry J. Grant, Westerville, OH (US);

Ronald A. Houpt, Newark, OH (US);

Teno Boone, Columbus, OH (US);

Toni Elwell Newsome, Pataskala, OH (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 33/02 (2006.01); C08F 20/06 (2006.01); C08K 3/40 (2006.01); C08K 7/14 (2006.01); C08L 29/04 (2006.01); C08L 29/14 (2006.01); E04B 1/76 (2006.01);
U.S. Cl.
CPC ...
C08L 33/02 (2013.01); C08F 20/06 (2013.01); C08K 3/40 (2013.01); C08K 7/14 (2013.01); C08L 29/04 (2013.01); C08L 29/14 (2013.01); E04B 1/7662 (2013.01); C08F 2810/20 (2013.01); C08L 2312/00 (2013.01);
Abstract

A fibrous insulation product comprising a plurality of randomly oriented glass fibers and a cross-linked formaldehyde-free binder composition at least partially coating the fibers is disclosed. The cross-linked formaldehyde-free binder composition is formed from an aqueous binder composition comprising 5.0% by weight to 37.0% by weight of at least one monomeric polyol having at least four hydroxyl groups and at least 50.0% by weight of a cross-linking agent comprising a polymeric polycarboxylic acid having at least two carboxylic acid groups, based on the total solids content of the aqueous binder composition. The glass fibers have an average fiber diameter in the range of 8 HT to 12 HT. The fibrous insulation product, after curing, has a density, when uncompressed, in the range of 0.30 pcf to 2.7 pcf.