The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 06, 2025

Filed:

Oct. 25, 2021
Applicant:

Foseco International Limited, Barlborough Links, GB;

Inventors:

Vincent Haanappel, Enschede, NL;

Thomas Linke, Enschede, NL;

Assignee:

FOSECO INTERNATIONAL LIMITED, Barlborough Links, GB;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22C 9/10 (2005.12); B22C 1/02 (2005.12); B22C 1/22 (2005.12); B22C 9/02 (2005.12); B22C 9/12 (2005.12); B22D 17/00 (2005.12); B22D 29/00 (2005.12); B33Y 10/00 (2014.12);
U.S. Cl.
CPC ...
B22C 1/22 (2012.12); B22C 1/02 (2012.12); B22C 9/10 (2012.12); B22C 9/12 (2012.12); B22D 17/007 (2012.12); B22D 29/002 (2012.12); B33Y 10/00 (2014.11);
Abstract

A composition for making a core for use in a moulding or casting process, a core comprising said composition, and a mould for producing an article by high pressure die casting or semi-solid casting. The composition comprises a particulate refractory material, a binder composition comprising at least one hydrophilic polymer, comprising at least one polysaccharide or polysaccharide derivative; and at least one pozzolanic additive. The mould comprises a core for defining an internal cavity of the article and the core comprises a solidified core composition. The solidified core composition comprises a particulate refractory material and a binder composition, degrades in water such that a cylinder of the solidified core composition having a maximum height of 80 mm and a maximum diameter of 50 mm disintegrates in no more than 10 minutes when immersed in water at a temperature of 20° C. and stirred at a speed of 60 rpm, and has a flexural strength of at least 300 N/cm. The invention also resides in a method for producing an article by high pressure die casting or semi-solid casting.