The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 29, 2025

Filed:

Jul. 26, 2023
Applicants:

PT Qmb New Energy Materials, Jakarta, ID;

PT Esg New Energy Material, Jakarta, ID;

Gem Co., Ltd., Shenzhen, CN;

PT Gem Indonesia New Energy Materials, Jakarta, ID;

Inventors:

Kaihua Xu, Shenzhen, CN;

Satryo Soemantri Brodjonegoro, Jakarta, ID;

Yi Wang, Jakarta, ID;

Rizky Wanaldi, Jakarta, ID;

Tegar Mukti Aji, Jakarta, ID;

Evan Wahyu Kristiyanto, Jakarta, ID;

Andi Syaputra Hasibuan, Jakarta, ID;

Piyan Rahmadi, Jakarta, ID;

Assignees:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C01G 53/10 (2005.12); C22B 3/08 (2005.12); C22B 3/24 (2005.12);
U.S. Cl.
CPC ...
C01G 53/10 (2012.12); C22B 3/08 (2012.12); C22B 3/24 (2012.12);
Abstract

The disclosure discloses a method for preparing a battery-grade nickel-cobalt-manganese sulfate solution from low nickel matte. The method includes the following steps: grinding low nickel matte, then adding the ground low nickel matte to concentrated sulfuric acid, and carrying out atmospheric pressure leaching to obtain a first slag phase and a first liquid phase; carrying out evaporation concentration-cooling crystallization on the first liquid phase to obtain ferrous sulfate crystals; adding concentrated sulfuric acid to the first slag phase, and carrying out oxygen pressure leaching to obtain a second slag phase and a second liquid phase; adjusting pH of the second liquid phase to 3-4 to generate a precipitate, and removing the precipitate by filtration to obtain a filtrate; carrying out adsorption treatment on the filtrate by adopting chelating resin; washing the adsorbed chelating resin with a first sulfuric acid solution to obtain a washing solution containing Mg and Mn, and then washing the chelating resin with a second sulfuric acid solution to obtain a nickel-cobalt sulfate solution; and mixing the nickel-cobalt sulfate solution with the washing solution containing Mg and Mn to obtain the nickel-cobalt-manganese sulfate solution. According to the method of the disclosure, the battery-grade nickel-cobalt sulfate solution is prepared from the low nickel matte as a raw material, so that the recovery rate of nickel and cobalt is increased, and the acid consumption is reduced.