The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 18, 2025

Filed:

Nov. 01, 2018
Applicant:

Celgard, Llc, Charlotte, NC (US);

Inventors:

Changqing Adams, Fort Mill, SC (US);

Geoffrey Allen Tice, Rock Hill, SC (US);

Gary Michael Shirah, Edgemoor, SC (US);

Assignee:

Celgard, LLC, Charlotte, NC (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 10/0569 (2010.01); H01M 50/417 (2021.01); H01M 50/451 (2021.01); H01M 50/457 (2021.01); H01M 50/489 (2021.01); H01M 50/491 (2021.01); H01M 50/494 (2021.01);
U.S. Cl.
CPC ...
H01M 10/0569 (2013.01); H01M 50/417 (2021.01); H01M 50/451 (2021.01); H01M 50/457 (2021.01); H01M 50/489 (2021.01); H01M 50/491 (2021.01); H01M 50/494 (2021.01); H01M 2300/0028 (2013.01);
Abstract

A microporous film having at least one of the following properties: unrestrained MD shrinkage, when the film is baked unrestrained at 90° C. for 1 hour, of 2% or more; unrestrained MD shrinkage, when the film is baked unrestrained at 105° C. for 1 hour, of 2.5% or more; MD restrained growth, when measured using the MD restrained growth test, of less than or equal to 0.2%; rebound or recovery of 5% or greater when measured by the compressibility test; a max compression greater than or equal to 18% when measured by the compressibility test; swelling in DEC when measured according to the swelling in DEC test of 0.95% or less; the film exhibits a round-shaped, not a slit-shaped opening when subjected to the puncture test; the lamellae of the film have a thickness no greater than 250 nm; a normalized puncture strength above 350 g/16 micron; and having higher modulus and lower elongation before break of less than 40% in the machine direction. Also disclosed is a battery separator, battery, or device comprising at least one microporous film as described herein.