The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 18, 2025

Filed:

Dec. 19, 2019
Applicant:

Pacific Industrial Development Corporation, Ann Arbor, MI (US);

Inventors:

Anatoly Bortun, Ypsilanti, MI (US);

Jin Cho, Utsunomiya, JP;

Yunkui Li, Ann Arbor, MI (US);

David Shepard, Canton, MI (US);

Mila Bortun, Ypsilanti, MI (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C01G 25/00 (2006.01); B01D 53/94 (2006.01); F01N 3/022 (2006.01); F01N 3/10 (2006.01); F01N 3/28 (2006.01);
U.S. Cl.
CPC ...
C01G 25/006 (2013.01); B01D 53/945 (2013.01); F01N 3/022 (2013.01); F01N 3/101 (2013.01); F01N 3/2803 (2013.01); B01D 2255/2061 (2013.01); B01D 2255/2063 (2013.01); B01D 2255/2065 (2013.01); B01D 2255/2066 (2013.01); B01D 2255/20715 (2013.01); B01D 2255/2092 (2013.01); B01D 2255/407 (2013.01); B01D 2255/908 (2013.01); B01D 2255/9202 (2013.01); B01D 2255/9205 (2013.01); B01D 2255/9207 (2013.01); C01P 2004/51 (2013.01); C01P 2004/61 (2013.01); C01P 2004/62 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); F01N 2370/04 (2013.01);
Abstract

A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine.