The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 04, 2025

Filed:

Aug. 27, 2018
Applicant:

Nanotek Instruments, Inc., Dayton, OH (US);

Inventors:

Hui He, Dayton, OH (US);

Aruna Zhamu, Springboro, OH (US);

Bor Z. Jang, Centerville, OH (US);

Assignee:

Honeycomb Battery Company, Dayton, OH (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/38 (2006.01); H01M 4/133 (2010.01); H01M 4/134 (2010.01); H01M 4/36 (2006.01); H01M 4/40 (2006.01); H01M 4/62 (2006.01); H01M 10/0525 (2010.01); H01M 10/42 (2006.01); H01M 4/02 (2006.01); H01M 4/86 (2006.01);
U.S. Cl.
CPC ...
H01M 4/382 (2013.01); H01M 4/133 (2013.01); H01M 4/134 (2013.01); H01M 4/366 (2013.01); H01M 4/405 (2013.01); H01M 4/622 (2013.01); H01M 4/624 (2013.01); H01M 10/0525 (2013.01); H01M 10/4235 (2013.01); H01M 2004/027 (2013.01); H01M 2004/028 (2013.01); H01M 2004/8684 (2013.01);
Abstract

The invention provides a method of improving the cycle-life of a lithium metal secondary battery. The method comprises implementing an anode-protecting layer between an anode active material layer and a porous separator/electrolyte, wherein the anode-protecting layer or cathode-protecting layer comprises a conductive sulfonated elastomer composite having from 0.01% to 40% by weight of a conductive reinforcement material and from 0.01% to 40% by weight of an electrochemically stable inorganic filler dispersed in a sulfonated elastomeric matrix material and the protecting layer has a thickness from 1 nm to 100 μm, a fully recoverable tensile strain from 2% to 500%, a lithium ion conductivity from 10S/cm to 5×10S/cm, and an electrical conductivity from 10S/cm to 100 S/cm when measured at room temperature.