The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 04, 2025

Filed:

Dec. 15, 2020
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Genki Abukawa, Tokyo, JP;

Masafumi Azuma, Tokyo, JP;

Eisaku Sakurada, Tokyo, JP;

Shohei Yabu, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); B32B 15/01 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/16 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/013 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/16 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); C22C 38/38 (2013.01); C21D 2211/008 (2013.01);
Abstract

This hot-rolled steel sheet has a predetermined chemical composition, a microstructure includes 80% or more of tempered martensite by a volume percentage and a remainder consisting of one or more of ferrite, pearlite, bainite, fresh martensite, and residual austenite, the tempered martensite includes 5×10pieces/mmor more of precipitates containing Ti and having an equivalent circle diameter of 5 nm or less per unit volume, in a surface layer region that is a range from a surface to a 1/10 position of a sheet thickness, a sum of an average pole density of a crystal orientation group consisting of {211}<111> to {111}<112> and a pole density in a crystal orientation of {110}<001> is 6.0 or less, and a tensile strength is 980 MPa or more.