The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 04, 2025

Filed:

Nov. 22, 2019
Applicant:

Baoshan Iron & Steel Co., Ltd., Shanghai, CN;

Inventors:

Wei Li, Shanghai, CN;

Xiaodong Zhu, Shanghai, CN;

Peng Xue, Shanghai, CN;

Assignee:
Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); C21D 1/26 (2006.01); C21D 6/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0263 (2013.01); C21D 1/26 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C21D 2211/004 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

Disclosed is a high-yield-ratio cold-rolled dual-phase steel, having the following chemical elements in percentage by mass: 0.05%-0.08% of C, 0.9%-1.2% of Mn, 0.1%-0.6% of Si, 0.030%-0.060% of Nb, 0.030%-0.060% of Ti, 0.015%-0.045% of Al, and the balance being Fe and other inevitable impurities. A manufacturing method for the high-yield-ratio cold-rolled dual-phase steel, comprising: (1) smelting and casting; (2) hot rolling, wherein a casting blank is controlled and soaked at a temperature of 1200° C.-1250° C.; rolled with the finish rolling temperature being 840° C.-930° C.; cooled at a speed of 20° C./s-70° C./s, and then wound at the winding temperature being 570° C.-630° C.; (3) cold rolling; (4) annealing at the soaking temperature being 750° C.-790° C. for 40 s-200 s, cooling at a speed of 30° C./s-80° C./s, the start temperature of cooling is 650° C. to 730° C., the aging temperature is 200° C. to 260° C., and the overaging time is 100 s to 400 s; and (5) leveling.