The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 28, 2025

Filed:

Jun. 24, 2019
Applicant:

Zeon Corporation, Tokyo, JP;

Inventors:

Maki Mesuda, Tokyo, JP;

Yukie Ito, Tokyo, JP;

Assignee:

ZEON CORPORATION, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/62 (2006.01); C08L 33/08 (2006.01); C08L 33/10 (2006.01); C08L 33/20 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/622 (2013.01); C08L 33/08 (2013.01); C08L 33/10 (2013.01); C08L 33/20 (2013.01); H01M 10/0525 (2013.01); C08L 2203/20 (2013.01); C08L 2207/53 (2013.01);
Abstract

Provided is a binder composition for an electrochemical device electrode with which it is possible to form an electrode mixed material layer that has excellent peel strength and dusting resistance and that can cause an electrochemical device to display excellent rate characteristics. The binder composition for an electrochemical device electrode contains a binder and an organic solvent. The binder includes a particulate polymer A and a polymer B. The particulate polymer A has a core-shell structure including a core portion and a shell portion at least partially covering an outer surface of the core portion, and a polymer forming the shell portion has a glass-transition temperature of −50° C. to 20° C. A mixture obtained by mixing the polymer B in a concentration of 8 mass % with the organic solvent has a viscosity at a shear rate of 1 sof 100 mPa·s to 10,000 mPa·s.