The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 14, 2025

Filed:

Jul. 27, 2020
Applicant:

Google Llc, Mountain View, CA (US);

Inventors:

Huijuan Chen, Fremont, CA (US);

Michael John Bliss, Santa Clara, CA (US);

Assignee:

Google LLC, Mountain View, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09K 5/14 (2006.01); C08K 3/04 (2006.01); C08K 3/08 (2006.01); C08K 3/22 (2006.01); H01L 23/373 (2006.01);
U.S. Cl.
CPC ...
C09K 5/14 (2013.01); C08K 3/04 (2013.01); C08K 3/08 (2013.01); C08K 3/22 (2013.01); H01L 23/3733 (2013.01); C08K 2003/0812 (2013.01); C08K 2003/2296 (2013.01); C08K 2201/001 (2013.01); C08K 2201/005 (2013.01);
Abstract

A method of making a thermal interface material includes: combining a powder of diamond particles having a nominal dimension of 1,000 nm or less with a volatile liquid hydrocarbon material to provide a diamond dispersion; and combining the diamond dispersion with a first mixture to provide the thermal interface material, wherein the first mixture includes a matrix material and particles of a first material have a nominal dimension in a range from 1 micron to 100 microns, and wherein the diamond particles compose 0.5 wt. % to 5 wt. % of the thermal interface material, the matrix material composes 10 wt. % or less of the thermal interface material, and the first material composes at least 40 wt. % of the thermal interface material.


Find Patent Forward Citations