The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 07, 2025

Filed:

Oct. 25, 2019
Applicant:

Toyobo Co., Ltd., Osaka, JP;

Inventors:

Mahiro Nakano, Inuyama, JP;

Masayuki Haruta, Inuyama, JP;

Assignee:

TOYOBO CO., LTD., Osaka, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29C 55/14 (2006.01); B29C 48/00 (2019.01); B29C 48/08 (2019.01); B29K 67/00 (2006.01); B29L 31/00 (2006.01); B29L 31/34 (2006.01); C08K 3/36 (2006.01);
U.S. Cl.
CPC ...
B29C 55/143 (2013.01); B29C 48/0018 (2019.02); B29C 48/08 (2019.02); C08K 3/36 (2013.01); B29C 2948/92704 (2019.02); B29K 2067/003 (2013.01); B29K 2995/0053 (2013.01); B29L 2031/3475 (2013.01); B29L 2031/712 (2013.01); C08K 2201/002 (2013.01);
Abstract

The present invention is to provide a method for producing a biaxially oriented polyester film that is superior in mechanical properties, transparency, and heat resistance, and at the same time, superior in secondary processing suitability and printing appearance. Disclosed is a biaxially oriented polyester film, having at least one surface satisfying the following requirements (1) and (2), and the film satisfying the following requirements (3) and (4). (1) A maximum peak height roughness (SRp) is 1.2 μm to 1.6 μm. (2) An arithmetic average roughness (SRa) is 0.024 μm to 0.045 μm. (3) A tensile strength in a longitudinal direction and a width direction is 180 MPa to 300 MPa. (4) A haze is 7% or less.