The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 24, 2024

Filed:

Oct. 19, 2018
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventor:

Seo Hee Ju, Daejeon, KR;

Assignee:

LG Chem, Ltd., Seoul, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); C01B 35/12 (2006.01); C01G 53/00 (2006.01); H01M 4/04 (2006.01); H01M 4/131 (2010.01); H01M 4/1391 (2010.01); H01M 4/505 (2010.01); H01M 4/62 (2006.01); H01M 10/052 (2010.01); H01M 10/0525 (2010.01); H01M 10/42 (2006.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); C01B 35/121 (2013.01); C01G 53/50 (2013.01); H01M 4/0471 (2013.01); H01M 4/131 (2013.01); H01M 4/1391 (2013.01); H01M 4/505 (2013.01); H01M 4/62 (2013.01); H01M 4/628 (2013.01); H01M 10/052 (2013.01); H01M 10/0525 (2013.01); H01M 10/4235 (2013.01); C01P 2004/80 (2013.01); C01P 2006/40 (2013.01); H01M 2004/028 (2013.01); H01M 2300/0008 (2013.01); H01M 2300/0011 (2013.01);
Abstract

A positive electrode active material includes a nickel-containing lithium transition metal oxide containing nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium, and a lithium-containing inorganic compound layer formed on a surface of the nickel-containing lithium transition metal oxide, wherein the positive electrode active material has a first peak in a range of 5 eV or less, a second peak in a range of 7 eV to 13 eV, and a third peak in a range of 20 eV to 30 eV when intensity is measured by X-ray photoelectron spectroscopy, and the first peak has a maximum value of 80% to 120% with respect to the third peak. A method of preparing the positive electrode active material, and a positive electrode and a lithium secondary battery are also provided.


Find Patent Forward Citations

Loading…