The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 24, 2024

Filed:

Apr. 24, 2019
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Masatoshi Aratani, Tokyo, JP;

Ryoji Matsui, Tokyo, JP;

Tomonori Kondo, Tokyo, JP;

Shinsaku Kokubo, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 6/00 (2006.01); B21C 37/08 (2006.01); B21D 7/025 (2006.01); B23K 11/08 (2006.01); B60G 21/055 (2006.01); C21D 8/10 (2006.01); C21D 9/08 (2006.01); C21D 9/50 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/42 (2006.01); C22C 38/50 (2006.01); C22C 38/54 (2006.01);
U.S. Cl.
CPC ...
B60G 21/055 (2013.01); B21C 37/0818 (2013.01); B21D 7/025 (2013.01); B23K 11/08 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/105 (2013.01); C21D 9/08 (2013.01); C21D 9/50 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/42 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01); B60G 2202/135 (2013.01); B60G 2206/012 (2013.01); B60G 2206/427 (2013.01); B60G 2206/724 (2013.01); B60G 2206/8103 (2013.01); B60G 2206/8402 (2013.01); B60G 2206/8403 (2013.01);
Abstract

An electric resistance welded steel pipe for manufacturing a hollow stabilizer has a Lankford value in a pipe longitudinal direction of from 0.7 to less than 1.0. The electric resistance welded steel pipe is subjected to cold bending and then to a heat treatment including quenching and tempering to manufacture a stabilizer. The cold bending is cold rotary draw bending. When bent with a bend radius of from 1.0 times to 3.0 times an outer diameter of the pipe before cold bending, a flattening ratio is from 0% to 10%, a thickness reduction rate on a bending outside and a thickness increase rate on a bending inside are from 0% to 10%, and additionally, a circumferential length change of a bending center portion is from 0% to 10%. A Vickers hardness of the stabilizer after the heat treatment is adjusted to from 400 HV to less than 580 HV.