The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 03, 2024

Filed:

Nov. 16, 2018
Applicants:

Dow Global Technologies Llc, Midland, MI (US);

Rohm and Haas Company, Collegeville, PA (US);

Inventors:

Chenyan Bai, Shanghai, CN;

Elodie Hablot, Horgen, CH;

Gaobing Chen, Shanghai, CN;

Thorsten Schmidt, Horgen, CH;

Abraham Barretto, Juinagar, IN;

Assignees:

Dow Global Technologies LLC, Midland, MI (US);

Rohm and Haas Company, Collegeville, PA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 175/14 (2006.01); C08G 18/32 (2006.01); C08G 18/40 (2006.01); C08G 18/42 (2006.01); C08G 18/48 (2006.01); C08G 18/62 (2006.01); C08G 18/66 (2006.01); C08G 18/72 (2006.01); C08G 18/73 (2006.01); C08G 18/76 (2006.01); C09J 5/00 (2006.01);
U.S. Cl.
CPC ...
C09J 175/14 (2013.01); C08G 18/3206 (2013.01); C08G 18/4063 (2013.01); C08G 18/4238 (2013.01); C08G 18/4829 (2013.01); C08G 18/627 (2013.01); C08G 18/6677 (2013.01); C08G 18/722 (2013.01); C08G 18/728 (2013.01); C08G 18/73 (2013.01); C08G 18/7671 (2013.01); C09J 5/00 (2013.01);
Abstract

A process comprises (i) providing an isocyanate component A that is a reaction product of an aliphatic polyisocyanate, an aromatic polyisocyanate, an aliphatic polyester polyol, and a polyether polyol; (ii) providing a polyol component B comprising an aliphatic polyester polyol and a polyether polyol; (iii) mixing A and B to form a solventless adhesive (SLA) composition component A and component B each comprises an aliphatic polyester polyol having a viscosity from 800 to 6000 mPa·s at 25° C. and a hydroxyl number from 60 to 180 mg KOH/g; the SLA composition has (a) an initial viscosity at 40° C. from 500 to 1600 mPa·s, (b) an increasing viscosity ratio from 100% to 112% of the initial viscosity after the SLA composition stands at 40° C. for 10 min, and (c) an end viscosity at 40° C. from 120% to 210% of the initial viscosity at 40 min after forming the SLA composition.