The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 12, 2024

Filed:

Sep. 12, 2019
Applicant:

Baoshan Iron & Steel Co., Ltd., Shanghai, CN;

Inventors:

Yuan Fang, Shanghai, CN;

Jianchun Wu, Shanghai, CN;

Jian Zhang, Shanghai, CN;

Assignee:
Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 9/52 (2006.01); B21B 1/22 (2006.01); B22D 11/06 (2006.01); B22D 11/116 (2006.01); B22D 11/124 (2006.01); C21D 1/667 (2006.01); C21D 8/02 (2006.01);
U.S. Cl.
CPC ...
C21D 9/52 (2013.01); B21B 1/22 (2013.01); B22D 11/0622 (2013.01); B22D 11/116 (2013.01); B22D 11/1246 (2013.01); C21D 1/667 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); B21B 2001/225 (2013.01);
Abstract

A method for producing ultra-thin hot-rolled strip steel, the method comprising the following process steps: A. a smelting process: feeding scrap steel into an induction electric furnace () for smelting so that the scrap steel melts into molten steel; B. a refining process: using a ladle refining furnace () and a ladle vacuum degassing furnace () to refine the molten steel; C. a continuous casting process: casting the refined molten steel into a cast strip blank that has a thickness of 1.6-2.5 mm by means of a dual-roller thin strip continuous casting system (); D. a hot rolling process: directly feeding the cast strip blank that was cast in the continuous casting process to a single-stand hot rolling mill () for rolling to produce hot-rolled strip steel, the thickness of the hot-rolled strip steel being 0.8-1.5 mm; E. a cooling coiling process: performing atomizing cooling on the hot-rolled strip steel, and coiling after the strip steel temperature is controlled to be 400-750° C. The present method achieves an extremely compact, environmentally-friendly and economical ultra-thin hot-rolled strip steel production process flow, and achieves the environmentally-friendly and economical continuous production of metal plates and strips.