The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 05, 2024

Filed:

Apr. 06, 2023
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Christian Allely, Metz, FR;

Pascal Bertho, Yutz, FR;

Anirban Chakraborty, Chesterton, IN (US);

Hassan Ghassemi-Armaki, Schererville, IN (US);

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/01 (2006.01); B23K 11/11 (2006.01); C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C23C 2/02 (2006.01); C23C 2/28 (2006.01); C23C 10/28 (2006.01); C25D 3/12 (2006.01); C25D 3/22 (2006.01); C25D 5/12 (2006.01); C25D 5/50 (2006.01);
U.S. Cl.
CPC ...
B32B 15/011 (2013.01); B23K 11/11 (2013.01); C21D 8/0273 (2013.01); C21D 9/46 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C23C 2/0224 (2022.08); C23C 2/28 (2013.01); C23C 10/28 (2013.01); C25D 3/12 (2013.01); C25D 3/22 (2013.01); C25D 5/12 (2013.01); C25D 5/50 (2013.01);
Abstract

The present invention relates to a method for the manufacture of a galvannealed steel sheet including the steps of A.) coating of the steel sheet with a first coating consisting of nickel and having a thickness between 150 nm and 650 nm, the steel sheet having the following composition in weight percentage 0.10<C<0.40%, 1.5<Mn<3.0%, 0.7<Si<3.0%, 0.05<Al<1.0%, 0.75<(Si+Al)<3.0%, and on a purely optional basis, one or more elements such as Nb≤0.5%, B≤0.010%, Cr≤1.0%, Mo≤0.50%, Ni≤1.0%, Ti≤0.5%., the remainder of the composition is made up of iron and inevitable impurities resulting from the elaboration, B.) annealing of the coated steel sheet being annealed at a temperature between 600 to 1200° C., C.) coating of the steel sheet obtained in step B.) with a second coating based on zinc and D.) an alloying heat treatment to form a galvannealed steel sheet.