The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 29, 2024

Filed:

Jul. 31, 2020
Applicant:

Hydromecanique ET Frottement, Andrezieux Boutheon, FR;

Inventors:

Sébastien Bucher, Saint Etienne, FR;

Christophe Gérard Pupier, Genas, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23F 1/00 (2006.01); B01J 13/04 (2006.01); B22F 1/065 (2022.01); B22F 1/145 (2022.01); B22F 1/17 (2022.01); B22F 10/28 (2021.01); B22F 10/34 (2021.01); B33Y 40/10 (2020.01); B33Y 70/00 (2020.01);
U.S. Cl.
CPC ...
B01J 13/04 (2013.01); B22F 1/065 (2022.01); B22F 1/145 (2022.01); B22F 1/17 (2022.01); B22F 10/28 (2021.01); B22F 10/34 (2021.01); B33Y 40/10 (2020.01); B33Y 70/00 (2014.12); B22F 2301/052 (2013.01); B22F 2301/10 (2013.01); B22F 2301/25 (2013.01); B22F 2304/10 (2013.01);
Abstract

The present invention relates to a method for preparing a metal powder intended for an additive manufacturing process, of the type that involves scanning a bed of powder by a near-infrared laser beam, characterized in that the method comprises: an initial step for selecting a powder, which has an optical reflectivity of higher than 70% for a wavelength ranging between 800 and 1500 nm; then a step for treating said powder, which is different from particle grafting, and which induces a physical and/or chemical surface modification of the grains of said powder, making it possible to lower its optical reflectivity, at the given wavelength. The invention also relates to the use of such a powder, the grains having, after treatment, a median grain size d50 of between 5 and 50 μm.