The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 08, 2024

Filed:

Apr. 18, 2023
Applicant:

Arcelormittal, Luxembourg, LU;

Inventor:

Hyun Jo Jun, Clinton, NJ (US);

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); B32B 15/01 (2006.01); C21D 1/20 (2006.01); C21D 1/25 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/26 (2006.01); C22C 38/38 (2006.01); C23C 2/02 (2006.01); C23C 2/06 (2006.01); C23C 2/28 (2006.01); C23C 2/40 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/013 (2013.01); C21D 1/20 (2013.01); C21D 1/25 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0247 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/26 (2013.01); C22C 38/38 (2013.01); C23C 2/02 (2013.01); C23C 2/022 (2022.08); C23C 2/06 (2013.01); C23C 2/28 (2013.01); C23C 2/29 (2022.08); C23C 2/40 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

A cold rolled, coated and post batch annealed steel sheet produced by a method is provided. The method includes cold rolling a steel sheet; coating the cold rolled steel sheet with a zinc or zinc alloy coating, the cold rolled, coated steel sheet having an initial hole expansion and an initial yield strength and post batch annealing the cold rolled, coated steel sheet at a tempering temperature in a range from 150 to 650° C., the post batch annealed steel sheet having a final hole expansion and a final yield strength. The steel sheet includes (in wt. %) C—0.1-0.3%, Mn—1-3%, Si—0.5-3.5%, Al—0.05-1.5% and Mo+Cr being between 0-1.0%. The final hole expansion is at least 80% greater than the initial hole expansion and the final yield strength is at least 30% greater than the initial yield strength.