The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 10, 2024

Filed:

Jan. 03, 2020
Applicants:

South China University of Technology, Guangdong, CN;

Guangdong Huayi Plumbing Fittings Industry Co., Ltd., Kaiping, CN;

Sun Yat-sen University Cancer Center, Guangdong, CN;

Inventors:

Chao Yang, Guangzhou, CN;

Haizhou Lu, Guangzhou, CN;

Yanfei Ding, Kaiping, CN;

Yuanyuan Li, Guangzhou, CN;

Jin Wang, Guangzhou, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 19/03 (2006.01); B22F 1/14 (2022.01); B22F 9/08 (2006.01); B23K 26/342 (2014.01); B33Y 10/00 (2015.01); B33Y 40/10 (2020.01); B33Y 70/00 (2020.01); C22C 1/04 (2023.01); C22C 19/00 (2006.01); B22F 10/28 (2021.01); B22F 10/34 (2021.01); B22F 10/36 (2021.01); B23K 103/14 (2006.01);
U.S. Cl.
CPC ...
C22C 19/03 (2013.01); B22F 1/14 (2022.01); B22F 9/082 (2013.01); B23K 26/342 (2015.10); B33Y 10/00 (2014.12); B33Y 40/10 (2020.01); B33Y 70/00 (2014.12); C22C 1/0433 (2013.01); C22C 19/007 (2013.01); B22F 2009/0836 (2013.01); B22F 10/28 (2021.01); B22F 10/34 (2021.01); B22F 10/36 (2021.01); B22F 2301/15 (2013.01); B22F 2304/10 (2013.01); B23K 2103/14 (2018.08);
Abstract

Disclosed are a 4D printing method and application of titanium-nickel shape memory alloy. The 4D printing method comprises the following steps: mixing and smelting pure titanium and pure nickel to obtain titanium-nickel alloy bars, then preparing alloy powder by a rotating electrode atomization method, and sieving the powder to obtain titanium-nickel alloy powder with a particle size of 15-53 μm; placing the obtained titanium-nickel alloy powder in a discharge plasma assisted ball mill for discharge treatment to perform surface modification of the powder; and subjecting the titanium-nickel alloy powder to SLM forming to obtain the titanium-nickel shape memory alloy.