The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 10, 2024

Filed:

Apr. 28, 2022
Applicant:

Totalenergies American Services, Inc., Houston, TX (US);

Inventors:

Russell McDonald, Humble, TX (US);

Michael McLeod, Houston, TX (US);

Fengkui Li, Houston, TX (US);

Theodore Harris, III, Houston, TX (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B65D 1/02 (2006.01); B29C 49/00 (2006.01); B29C 49/06 (2006.01); B29C 49/08 (2006.01); B29K 23/00 (2006.01); B29K 105/00 (2006.01); B29L 31/00 (2006.01);
U.S. Cl.
CPC ...
B65D 1/0207 (2013.01); B29C 49/0005 (2013.01); B29C 49/08 (2013.01); B65D 1/0223 (2013.01); B29C 49/06 (2013.01); B29K 2023/065 (2013.01); B29K 2105/0032 (2013.01); B29K 2105/0094 (2013.01); B29K 2995/0063 (2013.01); B29K 2995/0077 (2013.01); B29K 2995/0082 (2013.01); B29K 2995/0088 (2013.01); B29L 2031/7158 (2013.01); B65D 2501/0081 (2013.01);
Abstract

Disclosed is an injection stretch blow molded (ISBM) container containing a surface having a static coefficient of friction (COF) of 0.15 to 0.21, a dynamic COF of 0.06 to 0.1, wherein the surface retains a water contact angle of 76° or higher for up to three minutes after wetting of the surface with a water drop of 14 to 16 mm diameter and the container is made with a polymeric composition containing a high density polyethylene (HDPE) having a dispersity (Mw/Mn) of 9 or higher as measured by GPC; a MI2 of 1 g/10 min or higher as measured by ASTM D-1238; 190° C./2.16 kg, as measured by ASTM D-1238; and an environmental stress crack resistance (ESCR) at 100% Igepal of >150 hours as measured by ASTM D-1693, B.