The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 20, 2024

Filed:

Sep. 17, 2020
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Masato Yasuda, Tokyo, JP;

Takeo Aramaki, Tokyo, JP;

Shinya Yano, Tokyo, JP;

Yoshihiro Arita, Tokyo, JP;

Takashi Kataoka, Tokyo, JP;

Kenichi Murakami, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 1/147 (2006.01); C21D 6/00 (2006.01); C21D 8/00 (2006.01); C21D 8/12 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/16 (2006.01); C22C 38/34 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/005 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1283 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/16 (2013.01); C22C 38/34 (2013.01); H01F 1/147 (2013.01); C22C 2202/02 (2013.01);
Abstract

A grain-oriented electrical steel sheet comprises a base steel sheet and a glass coating that is formed on the surface of the base steel sheet, and is characterized in that: the base steel sheet contains as chemical components, in mass %, 0.010% or less of C, from 2.00% to 4.00% of Si, from 0.05% to 1.00% of Mn, from 0.010% to 0.065% of Al, 0.004% or less of N and 0.010% or less of S, with the balance of Fe and impurities, wherein the oxygen concentration in the glass coating and the base steel sheet is 2,500 ppm or less; and if Iis the first peak intensity of Al and Iis the second peak intensity of Al in the concentration profile of Al, the relationship of mathematical formula (1) I<Iis satisfied.