The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 06, 2024

Filed:

Aug. 05, 2020
Applicant:

Agc Inc., Chiyoda-ku, JP;

Inventors:

Masanobu Isshiki, Tokyo, JP;

Toru Ikeda, Tokyo, JP;

Yosuke Takeda, Tokyo, JP;

Takamichi Shimosaka, Tokyo, JP;

Takaaki Murakami, Tokyo, JP;

Assignee:

AGC Inc., Chiyoda-ku, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 7/023 (2019.01); G02B 1/11 (2015.01); G02B 1/115 (2015.01); G02B 5/02 (2006.01); G02F 1/1335 (2006.01);
U.S. Cl.
CPC ...
G02B 5/0294 (2013.01); G02B 1/11 (2013.01); G02B 1/115 (2013.01); G02B 5/0221 (2013.01); G02B 5/0236 (2013.01); G02B 5/0284 (2013.01); B32B 7/023 (2019.01); B32B 2307/40 (2013.01); G02F 1/133502 (2013.01); G02F 1/133504 (2013.01); G02F 2201/38 (2013.01); G02F 2203/03 (2013.01);
Abstract

A transparent substrate with an antiglare film, includes a transparent substrate having first and second main surfaces and an antiglare film formed on the first main surface. The antiglare film includes a low refractive index layer formed on the first main surface and a high refractive index layer formed in the low refractive index layer and having a refractive index different from that of the low refractive index layer. The low refractive index layer has nof 1.4 to 1.8. The high refractive index layer has nat least 0.1 higher than the n. The high refractive index layer has an area ratio of its portion where a surface inclination to the first main surface is 0.5° or less of 15% or less. An average length RSm of elements of a roughness curve of an outermost surface on a first main surface side is 50 μm or less.