The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 23, 2024

Filed:

Sep. 16, 2022
Applicant:

Material Sciences Corporation, Elk Grove Village, IL (US);

Inventors:

Peter Bortell, Tecumseh, MI (US);

Bryan Tullis, Livonia, MI (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 35/02 (2006.01); B32B 7/12 (2006.01); B32B 15/01 (2006.01); B32B 15/04 (2006.01); B32B 15/20 (2006.01); B32B 37/06 (2006.01); B32B 37/12 (2006.01); B23K 101/18 (2006.01);
U.S. Cl.
CPC ...
B23K 35/0255 (2013.01); B32B 7/12 (2013.01); B32B 15/01 (2013.01); B32B 15/016 (2013.01); B32B 15/04 (2013.01); B32B 15/043 (2013.01); B32B 15/20 (2013.01); B32B 37/06 (2013.01); B32B 37/12 (2013.01); B23K 2101/18 (2018.08); B32B 2255/06 (2013.01); B32B 2255/205 (2013.01); B32B 2264/101 (2013.01); B32B 2264/105 (2013.01); B32B 2264/107 (2013.01); B32B 2305/30 (2013.01); B32B 2307/10 (2013.01); B32B 2307/202 (2013.01); B32B 2311/24 (2013.01); B32B 2319/00 (2013.01);
Abstract

A laminate structure and method of forming is provided. The laminate structure includes a first metal sheet having a first thickness, a second metal sheet having a second thickness, and an adhesive core having an adhesive thickness. The adhesive core is disposed between and bonded to the first and second metal sheets. The first and second metal sheets are made of an aluminum based material and the adhesive core is made of an adhesive material also described as a viscoelastic adhesive material. The laminate structure is configured such that a ratio of the sum of the first and second thickness to the adhesive thickness is greater than either to one (8:1). The laminate structure including the viscoelastic adhesive core is characterized by a composite loss factor at 1,000 Hertz which is continuously greater than 0.1 within a temperature range of 25 degrees Celsius to 50 degrees Celsius.