The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 09, 2024

Filed:

Feb. 12, 2019
Applicant:

Winona Building Products, Llc, Etna Green, IN (US);

Inventors:

John F. Bergin, Wisconsin Rapids, WI (US);

James Herbert Stoken, Allegan, MI (US);

Assignee:

Winona Building Products, LLC, Etna Green, IN (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 5/18 (2006.01); B32B 7/12 (2006.01); C09J 7/38 (2018.01); C09J 11/04 (2006.01); C09J 11/06 (2006.01); C09J 11/08 (2006.01); C09K 21/04 (2006.01); E04B 1/76 (2006.01); E04B 1/94 (2006.01); H01B 3/18 (2006.01); C08K 3/22 (2006.01); C08K 3/32 (2006.01); E04B 1/74 (2006.01);
U.S. Cl.
CPC ...
C09K 21/04 (2013.01); B32B 7/12 (2013.01); C09J 7/383 (2018.01); C09J 11/04 (2013.01); C09J 11/06 (2013.01); C09J 11/08 (2013.01); E04B 1/7608 (2013.01); E04B 1/946 (2013.01); H01B 3/18 (2013.01); C08K 3/22 (2013.01); C08K 2003/2255 (2013.01); C08K 2003/2296 (2013.01); C08K 2003/321 (2013.01); C09J 2301/408 (2020.08); C09J 2401/00 (2013.01); C09J 2415/00 (2013.01); E04B 2001/742 (2013.01);
Abstract

An antimony-free adhesive package useful for making an insulation facing material includes a halogenated latex adhesive, a flame/smoke suppressant such as aluminum trihydrate, an intumescent such as aluminum polyphosphate, melamine powder, a melamine cyanurate, a mold and mildew inhibitor, an optional dispersant, an optional water holding agent, and optionally between 3% and 10% of a zinc molybdate/magnesium silicate complex and between 3% and 10% of a zinc phosphate/zinc oxide complex. Insulation facing material made with the adhesive package has a 'flame spread' value that does not exceed 25, and a “smoke developed” value that does not exceed 50, and meets the applicable standards for operating temperature, anti-corrosiveness, corrosion, puncture resistance, water vapor transmission, water vapor sorption, shrinkage, microbial growth resistance, and water immersion bond integrity. The facing stock may be used to face insulation products such as rolls, batts, boards or molds of fiberglass or mineral wool insulation.