The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 25, 2024

Filed:

Oct. 14, 2020
Applicant:

Agc Inc., Tokyo, JP;

Inventors:

Hirofumi Tokunaga, Tokyo, JP;

Kazutaka Ono, Tokyo, JP;

Motoyuki Hirose, Tokyo, JP;

Assignee:

AGC Inc., Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C03C 3/087 (2006.01); C03B 17/06 (2006.01); C03C 3/091 (2006.01); C03C 4/00 (2006.01);
U.S. Cl.
CPC ...
C03C 3/087 (2013.01); C03B 17/064 (2013.01); C03C 3/091 (2013.01); C03C 4/0085 (2013.01); C03C 2203/10 (2013.01);
Abstract

An alkali-free glass has a strain point of 650° C. or more, an average coefficient of thermal expansion at 50 to 350° C. of from 30×10to 45×10/° C., and a temperature Tat which a glass viscosity reaches 10dPa·s of from 1,500 to 1,800° C. The alkali-free glass contains, as represented by mol % based on oxides, SiO: from 62 to 70%, AlO: from 9 to 16% BO: from 0 to 12%, MgO: from 3 to 10%, CaO: from 4 to 12%, SrO: from 0 to 6%, and FeO: from 0.001 to 0.04%, provided that MgO+CaO+SrO+BaO is from 12 to 25%. The alkali-free glass has a β-OH value of from 0.35 to 0.85/mm.