The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 11, 2024

Filed:

Oct. 06, 2020
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Jun Ho Choe, Daejeon, KR;

Seung Cheol Ryoo, Daejeon, KR;

Seong Lyong Kim, Daejeon, KR;

Dae San Jung, Daejeon, KR;

Assignee:

LG CHEM, LTD., Seoul, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 25/12 (2006.01);
U.S. Cl.
CPC ...
C08L 25/12 (2013.01); C08L 2203/30 (2013.01); C08L 2205/035 (2013.01); C08L 2205/18 (2013.01); C08L 2207/066 (2013.01);
Abstract

The present invention provides a thermoplastic resin composition which comprises: a first polymer formed by graft polymerization of a diene-based rubber polymer with an aromatic vinyl-based monomer and a vinyl cyanide-based monomer; a second polymer comprising an aromatic vinyl-based monomer unit and a vinyl cyanide-based monomer unit; a third polymer formed by graft polymerization of an olefin-based polymer with an aromatic vinyl-based monomer and a vinyl cyanide-based monomer; and a fourth polymer comprising an olefin-based monomer unit and having a density of 0.92 to 0.94 g/cmas measured in accordance with ASTM D1505, a softening point of 100 to 120° C. as measured in accordance with ASTM D1525, and a melt flow index of 5 to 7 g/10 min as measured in accordance with ASTM D1238 at 190° C. and 2.16 kg, wherein the thermoplastic resin composition comprises the fourth polymer at 1 to 10 wt %.


Find Patent Forward Citations