The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 14, 2024

Filed:

Feb. 17, 2023
Applicant:

Posco Co., Ltd, Pohang-si, KR;

Inventors:

Sung-Il Kim, Gwangyang-si, KR;

Hyun-Taek Na, Gwangyang-si, KR;

Dong-Wan Kim, Gwangyang-si, KR;

Assignee:

POSCO CO., LTD, Pohang-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/58 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/58 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

Provided is a method for manufacturing a steel sheet, the method including: reheating a steel slab at a temperature of 1200° C. to 1350° C., the steel slab including, by weight %, carbon (C): 0.05% to 0.14%, silicon (Si): 0.01% to 1.0%, manganese (Mn): 1.5% to 2.5%, aluminum (Al): 0.01% to 0.1%, chromium (Cr): 0.005% to 1.0%, phosphorus (P): 0.001% to 0.05%, sulfur (S): 0.001% to 0.01%, nitrogen (N): 0.001% to 0.01%, niobium (Nb): 0.005% to 0.06%, titanium (Ti): 0.005% to 0.11%, and a balance of iron (Fe) and inevitable impurities; finish hot rolling the reheated steel slab under predetermined conditions to obtain a hot-rolled steel sheet; cooling the hot-rolled steel sheet at a cooling rate of 10° C./s to 100° C./s to a temperature of 400° C. to 500° C. after the finish hot rolling; and coiling the steel sheet at a temperature of 400° C. to 500° C. after the cooling.