The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 30, 2024

Filed:

Feb. 17, 2023
Applicant:

Posco Co., Ltd, Pohang-si, KR;

Inventors:

Tae-Jin Song, Gwangyang-si, KR;

Jeong-Eun Kim, Gwangyang-si, KR;

Chang-Sik Choi, Gwangyang-si, KR;

Assignee:

POSCO CO., LTD, Pohang-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0226 (2013.01); C21D 8/0205 (2013.01); C21D 8/0215 (2013.01); C21D 8/0247 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C21D 2211/001 (2013.01);
Abstract

Provided is a method of manufacturing a hot rolled steel sheet having excellent formability and fatigue properties, including: preparing a slab including, by weight %, 0.3 to 0.8% of carbon C, 13 to 25% of manganese (Mn), 0.1 to 1.0% of vanadium (V), 0.005 to 2.0% of silicon (Si), 0.01 to 2.5% of aluminum (Al), 0.03% or less of phosphorus (P), 0.03% or less of sulfur (S), 0.04% or less (excluding 0%) of nitrogen (N), and a remainder of iron (Fe) and inevitable impurities; heating the slab to 1050 to 1250° C.; finish rolling, the slab heated in the heating, at a temperature of not lower than a recrystallization temperature of a region having an average V concentration and not higher than a recrystallization temperature of a region having twice the average V concentration, to obtain a hot rolled steel sheet; and coiling the hot-rolled steel sheet at 50 to 700° C.


Find Patent Forward Citations

Loading…