The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 09, 2024

Filed:

Aug. 03, 2021
Applicants:

Guangdong Brunp Recycling Technology Co., Ltd., Foshan, CN;

Hunan Brunp Recycling Technology Co., Ltd., Changsha, CN;

Hunan Brunp Vehicles Recycling Co., Ltd., Changsha, CN;

Ningde Brunp Recycling Technology Co., Ltd., Ningde, CN;

Inventors:

Changdong Li, Foshan, CN;

Honghui Tang, Foshan, CN;

Chunyi Wang, Foshan, CN;

Xinan Pei, Foshan, CN;

Xingdui Li, Foshan, CN;

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C01G 53/10 (2006.01); C22B 1/06 (2006.01); C22B 3/00 (2006.01); C22B 3/08 (2006.01); C22B 3/38 (2006.01); C22B 23/00 (2006.01); C22B 23/02 (2006.01);
U.S. Cl.
CPC ...
C01G 53/10 (2013.01); C22B 1/06 (2013.01); C22B 3/08 (2013.01); C22B 3/3842 (2021.05); C22B 3/3844 (2021.05); C22B 3/3846 (2021.05); C22B 23/005 (2013.01); C22B 23/02 (2013.01); C22B 23/025 (2013.01); C22B 23/043 (2013.01); C22B 23/0453 (2013.01);
Abstract

Disclosed is a method for producing battery-grade nickel sulfate by using laterite nickel ore comprising the following steps: sorting the laterite nickel ore to obtain lump ore and sediment ore; crushing the lump ore, and then performing heap leaching, to obtain a crude nickel sulfate solution A; separating the sediment ore to obtain high chromium ore, low iron, high magnesium ore, and high iron, low magnesium ore, and drying, roasting, reducing, and sulfurating the low iron, high magnesium ore to obtain low nickel matte; blowing and performing water extraction on the low nickel matte, and then performing oxygen pressure leaching, to obtain a crude nickel sulfate solution B; performing pressure leaching on the high iron, low magnesium ore to obtain a crude nickel sulfate solution C; and performing extraction on the crude nickel sulfate solutions A, B, and C, and then evaporating and crystallizing, to obtain battery-grade nickel sulfate.