The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 02, 2024

Filed:

Jul. 23, 2020
Applicant:

Nanjing University of Aeronautics and Astronautics, Nanjing, CN;

Inventors:

Dongdong Gu, Nanjing, CN;

Kaijie Lin, Nanjing, CN;

Jingfeng Quan, Nanjing, CN;

Yamei Fang, Nanjing, CN;

Qing Ge, Nanjing, CN;

Jie Zhuang, Nanjing, CN;

Yang Liu, Nanjing, CN;

Weisong Dong, Nanjing, CN;

Pengjiang Shuai, Nanjing, CN;

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 38/00 (2006.01); B22F 1/05 (2022.01); B22F 1/065 (2022.01); B22F 9/04 (2006.01); B22F 10/28 (2021.01); B22F 10/322 (2021.01); B22F 10/36 (2021.01); B22F 10/366 (2021.01); B23K 26/00 (2014.01); B23K 26/342 (2014.01); B33Y 10/00 (2015.01); B33Y 70/00 (2020.01); B23K 103/04 (2006.01);
U.S. Cl.
CPC ...
C22C 38/007 (2013.01); B22F 9/04 (2013.01); B22F 10/28 (2021.01); B22F 10/36 (2021.01); B22F 10/366 (2021.01); B23K 26/0006 (2013.01); B23K 26/342 (2015.10); B33Y 70/00 (2014.12); B22F 1/05 (2022.01); B22F 1/065 (2022.01); B22F 2009/043 (2013.01); B22F 10/322 (2021.01); B22F 2301/255 (2013.01); B22F 2301/35 (2013.01); B22F 2304/10 (2013.01); B23K 2103/05 (2018.08); B33Y 10/00 (2014.12);
Abstract

The present disclosure relates to a micron silver particle-reinforced 316L stainless steel matrix composite, including a 316L stainless steel matrix and silver particles uniformly distributed in the 316L stainless steel matrix. The silver particles have a weight 1% to 5% of the total weight of the composite; and the composite has a density of 7.9 g/cmto 8.2 g/cmand a relative density of more than 98%. The composite is prepared by the following method: mixing raw materials of a spherical silver powder and a spherical 316L stainless steel powder; subjecting a resulting mixture to mechanical ball milling to obtain a mixed powder; sieving the mixed powder and adding a resulting powder to a powder cylinder of an SLM forming machine; and charging an inert protective gas for printing to obtain the composite.