The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 20, 2024

Filed:

Mar. 15, 2018
Applicant:

Jiapu Innovative Film (Kunshan) Co., Ltd., Jiangsu, CN;

Inventors:

Jialiang Xia, Suzhou, CN;

Xuewen Gao, Suzhou, CN;

Yu Xia, Suzhou, CN;

Minyan Tang, Suzhou, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 27/36 (2006.01); B32B 27/32 (2006.01); B65D 65/40 (2006.01); B32B 27/08 (2006.01); B32B 27/30 (2006.01); B32B 27/34 (2006.01);
U.S. Cl.
CPC ...
B32B 27/08 (2013.01); B32B 27/306 (2013.01); B32B 27/32 (2013.01); B32B 27/34 (2013.01); B32B 27/36 (2013.01); B65D 65/40 (2013.01); B32B 2250/05 (2013.01); B32B 2250/24 (2013.01); B32B 2307/518 (2013.01); B32B 2307/72 (2013.01); B32B 2553/00 (2013.01);
Abstract

A high-performance multilayer films for packaging and the structure of the multilayer film is as follows: PO2/POY/PO1/POX/PO3 and PO2/POY/PO1/TIE2/PO3. The multilayer film is obtained by multilayer coextrusion and biaxial stretching. The total thickness of the multilayer film is 8 to 100 micrometers; the absolute values of the differences of the solubility parameters between the PO1 layer and the PO2 layer and between the PO2 layer and PO3 layer is greater than 0.5 (J·cm), and the absolute value of the difference of the cohesive energy density is greater than 5 J/cm.