The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 06, 2024

Filed:

Jan. 26, 2022
Applicant:

Hitachi Metals, Ltd., Tokyo, JP;

Inventors:

Seiichi Kashimura, Tokyo, JP;

Masamichi Kishi, Tokyo, JP;

Naoto Teraki, Tokyo, JP;

Takanobu Watanabe, Tokyo, JP;

Yuriko Kiyokane, Tokyo, JP;

Assignee:

PROTERIAL, LTD., Tokyo, JP;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C09D 183/04 (2006.01); C09D 7/65 (2018.01); C09D 7/40 (2018.01); C09D 7/61 (2018.01); A61M 25/00 (2006.01); H01B 3/46 (2006.01); H01B 7/18 (2006.01); B32B 3/30 (2006.01); A61B 1/00 (2006.01); C08K 3/36 (2006.01);
U.S. Cl.
CPC ...
C09D 183/04 (2013.01); A61M 25/0045 (2013.01); B32B 3/30 (2013.01); C09D 7/61 (2018.01); C09D 7/65 (2018.01); C09D 7/69 (2018.01); H01B 3/46 (2013.01); H01B 7/18 (2013.01); A61B 1/00064 (2013.01); A61L 2420/04 (2013.01); A61M 2025/0046 (2013.01); C08K 3/36 (2013.01);
Abstract

A coating film is provided in a cable, a medical hollow tube, a molded article and a hollow tube. The coating film is formed from a rubber composition including a rubber component and fine particles. A static friction coefficient on a surface of the coating film is 0.5 or less. When the coating film is subjected to a testing such that a long fiber non-woven fabric including cotton linters including an alcohol for disinfection with a length of 50 mm along a wiping direction is brought contiguous to the surface of the coating film at a shearing stress of 2×10MPa to 4×10MPa, followed by wiping off the surface of the coating film at a speed of 80 times/min to 120 times/min and 20,000 repetitions thereof for a wiping direction length of 150 mm, a difference (an absolute value of a difference) between the static friction coefficients of the coating film before and after the testing is not greater than 0.1.