The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 16, 2024

Filed:

Jun. 25, 2020
Applicant:

Shipp Global Technologies B.v., Bergen op Zoom, NL;

Inventors:

Erik Schwartz, Bergen op Zoom, NL;

Sascha Jan ter Horst, Bergen op Zoom, NL;

Mark Adrianus Johannes van der Mee, Bergen op Zoom, NL;

Johannes Martinus Dina Goossens, Bergen op Zoom, NL;

Robert Dirk van de Grampel, Bergen op Zoom, NL;

Tony Farrell, Bergen op Zoom, NL;

Assignee:

SHPP GLOBAL TECHNOLOGIES B.V., Bergen op Zoom, NL;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 69/00 (2006.01); C08K 7/14 (2006.01); C08K 5/5399 (2006.01); C08J 5/04 (2006.01); C08G 64/08 (2006.01); C08J 9/00 (2006.01); C08K 5/00 (2006.01); C08K 5/521 (2006.01); C08L 27/18 (2006.01); C08L 83/04 (2006.01); C08K 5/523 (2006.01);
U.S. Cl.
CPC ...
C08J 5/043 (2013.01); C08G 64/085 (2013.01); C08J 9/009 (2013.01); C08K 5/0066 (2013.01); C08K 5/521 (2013.01); C08K 5/5399 (2013.01); C08K 7/14 (2013.01); C08L 27/18 (2013.01); C08L 69/00 (2013.01); C08L 69/005 (2013.01); C08L 83/04 (2013.01); C08K 5/523 (2013.01); C08L 2201/08 (2013.01); C08L 2203/20 (2013.01); C08L 2203/30 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01);
Abstract

A reinforced polycarbonate composition includes 30-60 wt % of a homopolycarbonate; 5-30 wt % of a poly(carbonate-siloxane); 10-40 wt % of a high heat polycarbonate having a glass transition temperature of 170° C. or higher determined per ASTM D3418 with a 20° C./min heating rate; 1-10 wt % of a phosphorous-containing flame retardant present in amount effective to provide 0.1-1.5 wt % phosphorous; 0.01-0.5 wt % of an anti-drip agent; 5-30 wt % of a reinforcing fiber; and optionally, up to 10 wt % of an additive composition, wherein each amount is based on the total weight of the reinforced polycarbonate composition, which sums to 100 wt %. A molded sample of the polycarbonate composition has a heat deflection temperature greater than 115° C., preferably greater than 125° C., more preferably greater than 130° C., or a flame test rating of V1, preferably V0 as measured according to UL-94 at a thickness of 0.8 millimeter, or at a thickness of 0.6 mm, or at a thickness of 0.4 mm.