The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 16, 2024

Filed:

Aug. 30, 2018
Applicant:

Central South University, Hunan, CN;

Inventors:

Zuming Liu, Hunan, CN;

Kai Peng, Hunan, CN;

Xueqian Lv, Hunan, CN;

Fan Zhao, Hunan, CN;

Quan Li, Hunan, CN;

Bing Wei, Hunan, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 10/28 (2021.01); B22F 3/24 (2006.01); B22F 10/36 (2021.01); B22F 10/366 (2021.01); B22F 10/38 (2021.01); B22F 10/64 (2021.01); B22F 1/052 (2022.01); B33Y 10/00 (2015.01); B33Y 40/20 (2020.01); B22F 3/105 (2006.01); B22F 12/17 (2021.01); B22F 10/32 (2021.01);
U.S. Cl.
CPC ...
B22F 10/28 (2021.01); B22F 1/052 (2022.01); B22F 3/24 (2013.01); B22F 10/36 (2021.01); B22F 10/366 (2021.01); B22F 10/38 (2021.01); B22F 10/64 (2021.01); B22F 10/32 (2021.01); B22F 12/17 (2021.01); B22F 2003/1051 (2013.01); B22F 2003/248 (2013.01); B22F 2301/15 (2013.01); B22F 2304/10 (2013.01); B33Y 10/00 (2014.12); B33Y 40/20 (2020.01);
Abstract

The present disclosure relates to the field of additive manufacturing and superalloys, particularly to a method for eliminating cracks in René 104 nickel-based superalloy prepared by laser additive manufacturing. For solving the problem that cracks are easily generated during laser additive manufacturing of René 104 nickel-based superalloy with high content of Al and Ti (Al+Ti>5 wt. %), generation of large-size cracks inside a fabricated part is suppressed by means of designing laser forming parameters and a partition scanning strategy; then stress relief annealing is performed to completely eliminate residual stress inside the fabricated part; and a spark plasma sintering process is performed to eliminate cracks inside the fabricated part and suppress the growth of grains during the sintering process.


Find Patent Forward Citations

Loading…