The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 26, 2023

Filed:

Jun. 29, 2021
Applicant:

Nichia Corporation, Anan, JP;

Inventors:

Toshiyuki Hirai, Komatsushima, JP;

Keisuke Suzuki, Anan, JP;

Hirofumi Oguri, Komatsushima, JP;

Assignee:

NICHIA CORPORATION, Anan, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/10 (2006.01); C04B 35/64 (2006.01); C04B 35/44 (2006.01); C09K 11/77 (2006.01); C04B 35/117 (2006.01); C04B 35/645 (2006.01); C04B 111/80 (2006.01);
U.S. Cl.
CPC ...
C04B 35/10 (2013.01); C04B 35/117 (2013.01); C04B 35/44 (2013.01); C04B 35/64 (2013.01); C04B 35/6455 (2013.01); C09K 11/7774 (2013.01); C04B 2111/807 (2013.01); C04B 2235/3222 (2013.01); C04B 2235/3224 (2013.01); C04B 2235/3225 (2013.01); C04B 2235/3227 (2013.01); C04B 2235/661 (2013.01); C04B 2235/662 (2013.01); C04B 2235/77 (2013.01); C04B 2235/78 (2013.01); C04B 2235/786 (2013.01); C04B 2235/963 (2013.01);
Abstract

A method for producing a ceramic complex includes: preparing a raw material mixture that contains 5% by mass or more and 40% by mass or less of first rare earth aluminate fluorescent material particles containing an activating element and a first rare earth element different from the activating element, 0.1% by mass or more and 32% by mass or less of oxide particles containing a second rare earth element, and the balance of aluminum oxide particles, relative to 100% by mass of the total amount of the first rare earth aluminate fluorescent material particles, the oxide particles, and the aluminum oxide particles; preparing a molded body of the raw material mixture; and obtaining a sintered body by calcining the molded body in a temperature range of 1,550° C. or higher and 1,800° C. or lower.