The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 26, 2023

Filed:

Aug. 27, 2020
Applicants:

Gary L. Anderson, St. Marys, PA (US);

Peter Stauffer, St. Marys, PA (US);

Inventors:

Gary L. Anderson, St. Marys, PA (US);

Peter Stauffer, St. Marys, PA (US);

Assignee:

Keystone Powdered Metal Company, St. Marys, PA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 3/16 (2006.01); C22C 38/08 (2006.01); B22F 3/17 (2006.01); B22F 1/00 (2022.01); C22C 38/16 (2006.01); C22C 38/12 (2006.01); B22F 5/08 (2006.01); F16H 55/17 (2006.01);
U.S. Cl.
CPC ...
B22F 3/16 (2013.01); B22F 1/0003 (2013.01); B22F 3/17 (2013.01); B22F 5/08 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/16 (2013.01); F16H 55/17 (2013.01); B22F 2301/10 (2013.01); B22F 2301/15 (2013.01); B22F 2301/20 (2013.01); B22F 2301/35 (2013.01); B22F 2302/40 (2013.01); F16H 2055/176 (2013.01);
Abstract

By utilizing the technique of this invention, parts such as gears, bearing races, and one-way clutches, which could previously only be made via labor intensive machining procedures can be made utilizing power metal technology. The subject invention provides a method of manufacturing a high strength part which comprised (1) providing an external component having an external profile and an internal profile, wherein the external component is comprised of a forged powder metal or a wrought metal; (2) compacting a powder metal composition within the internal profile of the external component to produce a green internal component having a desired internal profile; and (3) sintering the green internal component within the confines of the external component to produce high strength part, and wherein the internal component is comprised of a powder metal which expands to a greater degree than does the forged power metal or the wrought metal during sintering.