The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Nov. 28, 2023
Filed:
Sep. 17, 2015
Applicant:
Mitsubishi Rayon Co., Ltd., Tokyo, JP;
Inventor:
Osamu Okunaka, Tokyo, JP;
Assignee:
MITSUBISHI CHEMICAL CORPORATION, Tokyo, JP;
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29C 48/05 (2019.01); B29B 9/06 (2006.01); B29B 9/14 (2006.01); B29B 11/16 (2006.01); B29C 43/22 (2006.01); B29C 48/12 (2019.01); B29C 48/16 (2019.01); B29C 48/92 (2019.01); B29C 70/50 (2006.01); B29B 7/90 (2006.01); B29B 15/12 (2006.01); B29C 48/00 (2019.01); B29C 48/04 (2019.01); B29C 48/35 (2019.01); B29K 101/12 (2006.01); B29K 105/08 (2006.01); B29K 307/04 (2006.01);
U.S. Cl.
CPC ...
B29C 48/05 (2019.02); B29B 9/06 (2013.01); B29B 9/14 (2013.01); B29B 11/16 (2013.01); B29C 43/22 (2013.01); B29C 48/12 (2019.02); B29C 48/16 (2019.02); B29C 48/92 (2019.02); B29C 70/50 (2013.01); B29B 7/90 (2013.01); B29B 15/122 (2013.01); B29C 48/0011 (2019.02); B29C 48/04 (2019.02); B29C 48/35 (2019.02); B29C 2948/92523 (2019.02); B29K 2101/12 (2013.01); B29K 2105/0881 (2013.01); B29K 2307/04 (2013.01);
Abstract
A production method for a fiber-reinforced thermoplastic resin composite material, the method using a crosshead die () that has a maximum aperture height of 1 mm or more, wherein reinforcing fibers are supplied in a reinforcing fiber bundle to the crosshead die (), the reinforcing fibers are conjugated with a melted thermoplastic resin, and the conjugate is brought into contact with a pressurization surface that is at or below the solidification temperature of the thermoplastic resin, is pressurized, and is shaped to have a thickness that is 50% or less of the aperture height.