The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 21, 2023

Filed:

Oct. 31, 2018
Applicant:

Nec Corporation, Tokyo, JP;

Inventor:

Takeshi Azami, Tokyo, JP;

Assignee:

NEC CORPORATION, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); H01M 4/131 (2010.01); H01M 4/1391 (2010.01); H01M 4/36 (2006.01); H01M 4/62 (2006.01); H01M 10/0525 (2010.01); H01M 4/02 (2006.01); H01M 4/505 (2010.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); H01M 4/131 (2013.01); H01M 4/1391 (2013.01); H01M 4/366 (2013.01); H01M 4/505 (2013.01); H01M 4/623 (2013.01); H01M 4/625 (2013.01); H01M 10/0525 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01); H01M 2220/20 (2013.01); Y02E 60/10 (2013.01);
Abstract

A purpose of the present invention is to provide a lithium ion secondary battery having more improved life characteristics while suppressing gelation of an electrode mixture slurry in a manufacturing process. The lithium ion secondary battery according to the present invention comprises a positive electrode having a positive electrode mixture layer comprising a layered lithium-nickel composite oxide in which a proportion of nickel in metals other than lithium is 80 mol % or more; LiOH; LiCO; and a chlorine-containing polyvinylidene fluoride-based polymer, wherein a content of LiOH in the positive electrode mixture layer and a content of LiCOin the positive electrode mixture layer are each 0.1 weight % or more and 2.1 weight % or less, a total content of LiOH and LiCOin the positive electrode mixture layer is 0.2 weight % or more and 4.2 weight % or less, and a content of chlorine in the positive electrode mixture layer is 30 μg/g or more and 120 μg/g or less.