The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 07, 2023

Filed:

Jun. 08, 2018
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Masaki Ueyama, Tokyo, JP;

Yusaku Tomio, Tokyo, JP;

Yuhei Suzuki, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/08 (2006.01); C21D 6/00 (2006.01); C21D 8/10 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01);
U.S. Cl.
CPC ...
C21D 9/08 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/105 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C21D 2211/001 (2013.01);
Abstract

Provided is an austenitic alloy pipe, which has high yield strength, excellent SCC resistance, suppressed strength anisotropy, and high detectability in ultrasonic flaw detection. The austenitic alloy pipe according to the present embodiment has a chemical composition consisting of: in mass %, C: 0.004 to 0.030%, Si: 1.00% or less, Mn: 0.30 to 2.00%, P: 0.030 or less, S: 0.0020% or less, Al: 0.001 to 0.100%, Cu: 0.50 to 1.50%, Ni: 25.00 to 55.00%, Cr: 20.00 to 30.00%, Mo: 2.00 to 10.00%, and N: 0.005 to 0.100%, with the balance being Fe and impurities. A grain size number of austenite crystal grain is 2.0 to 7.0 and a mixed grain ratio is not more than 5%. Tensile YS is not less than 758 MPa, compressive YS/tensile YS is 0.85 to 1.10, and an outer diameter is not less than 170 mm.


Find Patent Forward Citations